dc.description | วารสารวิชาการและวิจัย มทร.พระนคร, 13(1) : 51-62 | en_US |
dc.description.abstract | The hybrid materials of lead sulfide with montmorillonite were synthesized by a solid-solid reaction between lead-exchanged montmorillonite and sodium sulfide at ambient condition. The hybrids were characterized by powder X-ray diffraction (XRD), thermogravimetric-differential thermal analysis (TG-DTA).The basal spacing of heat-treated lead sulfide-montmorillonite-sodium sulfide (200oC) was 1.20 nm. The formation of lead sulfide in the hybrid confirmed by the non-resolved absorption band and absorption onset at 328 and 508 nm, respectively for heat-treated lead sulfide-montmorillonite-sodium sulfide. The dramatic blue-shifted in the absorption onset relative to that of bulk was observed.The heat treated lead sulfide-montmorillonite-sodium sulfide showed an emission peak at 367 nm. The removal of adsorbed water resulted in the increasing intensity of the hybrid. | en_US |
dc.description.sponsorship | Rajamangala University of Technology Phra Nakhon | en_US |
dc.language.iso | th | en_US |
dc.subject | Montmorillonite | en_US |
dc.subject | มอนต์มอริลโลไนต์ | en_US |
dc.subject | Solid-solid Reaction | en_US |
dc.subject | ปฏิกิริยาที่เป็นของแข็ง | en_US |
dc.subject | Lead Sulfide | en_US |
dc.subject | ตะกั่วซัลไฟด์ | en_US |
dc.subject | Optical Properties | en_US |
dc.subject | คุณสมบัติทางแสง | en_US |
dc.title | A simple solid-solid reaction for the synthesis of lead sulfide-montmorillonite hybrid | en_US |
dc.type | Journal Articles | en_US |
dc.contributor.emailauthor | ontamareeporn@yahoo.com | en_US |
dc.contributor.emailauthor | arit@rmutp.ac.th | en_US |